5052 Vs 5083 Aluminum Plate: Which Aluminum Plate Should You Choose?

Oct 13, 2026

Leave a message

5052 and 5083 are the two workhorse non-heat-treatable 5xxx aluminum plates. Both gain strength from magnesium in solid solution, both weld cleanly, and both resist corrosion - but 5083 carries roughly double the magnesium and is built for seawater and welded marine structure, while 5052 is the general-purpose forming grade. This page compares them with numbers, not adjectives.

 

Scope: values shown for 5052-H32 and 5083-H116 (the structural tempers most often quoted for plate). Mechanical figures follow ASTM B209, EN 485-2 and GB/T 3880; 5083 marine plate is also supplied to ASTM B928 (H116/H321, exfoliation-tested). Final acceptance is by MTC.

Send an Inquiry Now

5052 vs 5083 Aluminum Plate Comparison Table

Every cell is a comparable figure for the stated temper. Rows marked indicative are typical workshop ranges, not guaranteed specification minima.

Metric 5052-H32 5083-H116
Tensile strength, UTS (MPa) 215–265 ≥305
Yield strength, Rp0.2 (MPa) ≥160 ≥215
Elongation at break (%) ≥7 ≥10
Magnesium, Mg (%) 2.2–2.8 4.0–4.9
Manganese, Mn (%) ≤0.10 0.40–1.0
Chromium, Cr (%) 0.15–0.35 0.05–0.25
Density (g/cm³) 2.68 2.66
Welded joint efficiency (typical % of parent UTS) ~90 (5356 filler) ~90 (5183/5356 filler)
Relative machinability (free-cutting brass = 100) 50 (indicative) 45 (indicative)
Relative cost (index) 100 (base) 108–112 (+8–12% indicative, market-dependent)
Best for General corrosion-resistant structures, fuel tanks, vehicle bodies, cladding Ship/marine welded structures, pressure vessels, cryogenic tanks, heavy plate

Standards referenced: ASTM B209 (plate/sheet), EN 485-2 / EN 573-3 (EN properties/composition), GB/T 3880, and ASTM B928 for 5083 marine plate (H116/H321).

 

5083 Aluminum Plate

 

Aluminum Strength and Formability: 5052 vs 5083 Aluminum Plate

The strength gap is set by magnesium content: 5083 carries 4.0–4.9% Mg against 5052's 2.2–2.8%.

Yield: 5083-H116 holds ≥215 MPa, about 55 MPa above 5052-H32's ≥160 MPa. In UTS the gap is ~40 MPa (≥305 vs 215–265).

Ductility: 5083-H116 still reaches ≥10% elongation; 5052-H32 is ≥7%. In the soft O condition, 5052 runs ~19–25% elongation vs 5083-O ~16–20% (indicative) - 5052 draws and bends more easily.

Formability drivers: higher Mg makes 5083 stiffer and less formable; 5052 is the grade chosen when the plate is spun, deep-drawn, folded or routed. 5083 is chosen when the plate is cut, welded and stiffened, not formed.

 

Aluminum Corrosion Resistance: 5052 vs 5083 aluminum alloy Plate

Both are non-heat-treatable 5xxx grades with a stable, self-healing oxide film and excellent general corrosion resistance. The selection line is the service environment:

Seawater / marine: 5083 (Mg 4.0–4.9%) is the marine-standard plate and is supplied H116/H321 to ASTM B928, which qualifies it against exfoliation and intergranular corrosion in seawater. 5052 is fine in splash/atmospheric marine but is not the grade for continuously wetted hull or ballast structure.

General atmosphere / fluids: 5052 (Mg 2.2–2.8%) is more than adequate for fuel tanks, vehicle panels, architectural cladding and food/chemical vessels at moderate temperature, and its higher formability offsets the lower strength.

Temperature limit: both are used cryogenically (5083 is common in LNG/tank service); sustained service above ~65 °C for high-Mg 5xxx should be reviewed for sensitization - confirm with the spec for the exact temper.

 

Aluminum Weldability and Machining: 5052 vs 5083 Plate

Both are non-heat-treatable, so welding does not soften a hardened zone the way it does for 6xxx - this is their key advantage over 6061/6082 in fabricated structures.

Welded joint efficiency: ~90% of parent UTS with the right filler - 5356 for 5052, 5183 / 5356 for 5083 marine welds (indicative). The welded assembly keeps most of its strength because there is no precipitation hardening to lose.

Process: MIG/TIG both work; 5083 marine joints are typically 5183 to match the higher Mg and keep corrosion parity in the weld. Post-weld stress relief is not usually required for either grade.

Machining: both machine at about 45–50% of free-cutting brass (indicative); 5083 is slightly gummier (higher Mg) and needs sharper geometry and coolant, but neither is difficult on standard equipment.

 

5083 h116 BV NR216 6x2000x6000 Aluminum Alloy Plate MTC

 

Aluminum Cost Difference: 5052 vs 5083 Plate

5083-H116 typically costs +8–12% more than 5052-H32 (indicative, market-dependent - Mg content, marine qualification to ASTM B928 and plate thickness all move the premium). The premium buys seawater qualification and ~55 MPa more yield. For atmospheric or formed parts, 5052 at base cost is the rational default; for welded marine or pressure service, 5083's premium removes a later cladding or over-design step.

Cost driver 5052-H32 5083-H116 Price effect (indicative)
Magnesium content (costliest common alloying metal) 2.2–2.8% 4.0–4.9% +3–4% ~2 pts more Mg
Temper / process route H32 (strain-hardened, no heat treat) H116 (stress-relieved + exfoliation-checked) +2–3% extra process + inspection
Marine qualification General EN 485 / ASTM B209 ASTM B928 + DNV/BV/ABS/CCS +2–4% class-society cert + 3rd-party test
Composite relative price index 100 (base) 108–112 +8–12% indicative, market-dependent

 

When to Choose 5052 or 5083 Aluminum Plate

Choose 5052-H32 when

The part is formed, bent, spun or deep-drawn (higher elongation, tighter bend radius).

Service is atmospheric, fuel/tank, vehicle body or architectural - not continuously wetted seawater.

You want the lowest plate cost that still gives good corrosion resistance and weldability.

Choose 5083-H116 when

The structure is ship hull, deck, offshore, ballast or other continuously wetted marine service (specify to ASTM B928 H116/H321).

You need ≥215 MPa yield in a welded plate without post-weld strength loss.

The job is a pressure vessel, cryogenic tank or heavy fabricated structure where 5052's yield is short.

 

FAQ: 5052 vs 5083 Aluminum Plate

Q: Is 5083 stronger than 5052?
A: Yes, in every temper comparison - 5083-H116 yield is ≥215 MPa vs 5052-H32 ≥160 MPa (about 55 MPa higher), driven by its 4.0–4.9% Mg against 5052's 2.2–2.8%.

Q: Can 5052 replace 5083 for marine use?
A: Not for hull, ballast or continuously wetted seawater structure - 5083 is qualified to ASTM B928 (H116/H321) for exfoliation resistance. 5052 is acceptable for splash zones and atmospheric marine but is not the marine-grade plate.

Q: Which aluminum plate welds better?
A: Both weld to ~90% joint efficiency (indicative) with no HAZ softening because they are non-heat-treatable; 5052 uses 5356 filler, 5083 uses 5183/5356 for marine parity. Both beat heat-treatable 6xxx on as-welded strength retention.

Q: Which is cheaper?
A: 5052-H32 is the base (index 100); 5083-H116 runs about +8–12% indicative, market-dependent.

 

Compare 5052 and 5083 Aluminum Plate and Request a Quote

Send your temper, plate dimensions (thickness × width × length), quantity and standard (ASTM B209 or ASTM B928 for marine 5083), and we will return availability and pricing for both grades.

Request a Quote

GNEE stocks 5052 and 5083 plate with EN 10204 3.1 mill certificate; marine 5083 H116/H321 to ASTM B928 available, 3.2 and third-party inspection on request.

 

About GNEE Aluminum Supply

GNEE stocks 5xxx aluminum plate - 5052 and 5083 - in common gauges and widths, with marine-grade 5083 H116/H321 available to ASTM B928. Operating since 2008 and exporting to 100+ countries, we handle both small and large orders with flexible MOQ and 15–30 day lead time. Each plate ships with an EN 10204 3.1 MTC; our team advises temper and alloy by service environment - atmospheric versus seawater, formed versus welded - so the plate you receive matches the job, not just the drawing.

Request Latest Price