First, the scrap aluminum is classified into primary categories and stacked in different grades, such as pure aluminum, deformed aluminum alloy, cast aluminum alloy, mixed materials, etc.
Iron impurities are very harmful to the smelting of scrap aluminum. When there is too much iron, brittle metal crystals will be formed in the aluminum, thereby reducing its mechanical properties and weakening its corrosion resistance. The iron content should generally be controlled below 1.2%. Scrap lead with an iron content of more than 1.5% can be used as a deoxidizer in the steel industry. Commercial aluminum alloys rarely use scrap aluminum with high iron content for smelting.

Scrap aluminum often contains organic non-metallic impurities such as paint, oil, plastic, rubber, etc. It must be removed before returning to the furnace for smelting. For wire scrap aluminum, the foreskin can generally be removed by mechanical grinding or shear stripping, heating stripping, chemical stripping and other measures.
For aluminum foil paper, it is difficult to effectively separate the aluminum foil layer and the paper fiber layer using ordinary waste paper pulping equipment. An effective separation method is to first place the aluminum foil paper in an aqueous solution, heat and pressurize it, and then quickly discharge it to a low-pressure environment for decompression. , and perform mechanical stirring. This separation method can recycle both fiber pulp and aluminum foil.

The liquefaction and separation of scrap aluminum is the future development direction for recycling metallic aluminum. It combines the pretreatment of scrap aluminum miscellaneous materials with re-melting and casting, which not only shortens the process flow, but also avoids air pollution to the greatest extent, and enables the recovery of clean metal. The rate is greatly improved.
There is a filter in the device that allows gas particles to pass through. In the liquefied layer, aluminum precipitates at the bottom. The paint and other organic matter attached to the scrap aluminum decomposes into gas, tar and solid carbon above 450°C, and then passes through the oxidation device inside the separator. Burn completely. The waste material is stirred by the rotating drum and mixed with the dissolving liquid in the bin. Impurities such as sand and gravel are separated into the sand and gravel separation area. The dissolving material brought out by the waste material returns to the liquefaction bin through the recovery propeller.