Aluminum Alloy Casting

Jan 12, 2024

Leave a message

Casting generally adopts vertical or horizontal water-cooled semi-continuous casting method. In order to improve the ingot structure and surface quality of vertical casting, electromagnetic crystallization tank, short crystallization tank and hot top casting method have also been developed (see solidification of metal). The water-cooled semi-continuous casting method introduces liquid metal into a water-cooled crystallizer through a launder, so that the liquid metal is cooled to form a solidified shell, which is pulled out of the crystallizer by the base of the casting machine or evenly dropped by its own weight to form an ingot.

Flexible Packaging Aluminum Foil For Cheese,milk/cream Ca...

 

Process parameters vary greatly depending on alloy composition and billet size. Generally, the casting speed and cooling rate should be increased as much as possible, and the height of the crystallization tank should be reduced. The casting temperature is usually 50 to 110°C higher than the liquidus of the alloy. In addition, the continuous casting and rolling process of aluminum plate and strip has also been developed. Plate and strip production adopts flat roll rolling, and the basic processes are hot rolling, cold rolling, heat treatment and finishing. For hard aluminum alloys such as LY12 and LC4 with complex chemical compositions, they should be homogenized before hot rolling. The treatment temperature is generally 10 to 15°C lower than the eutectic temperature of the low melting point phase in the alloy, and the temperature is kept for 12 to 24 hours. The aluminum-clad hard aluminum alloy is placed on both sides of the milled billet and welded by hot rolling. The thickness of the aluminum cladding layer is generally 4% of the plate thickness.