1. Raw material smelting
Batching and smelting
According to the target alloy model (such as 6063, 7000 series), calculate the ratio of aluminum ingots and alloy elements (magnesium, silicon, copper, etc.), and put the raw materials into the smelting furnace for high-temperature melting.
The impurities and gases in the aluminum liquid are removed through degassing and slag removal processes to ensure the purity of the material.
Casting
The refined aluminum liquid is injected into the casting machine and cooled into cylindrical cast bars (round cast bars) as the raw material for subsequent extrusion.
2. Mold design and extrusion molding
Mold design
Design the mold according to the cross-sectional shape requirements of the profile, and use CNC milling machines or EDM to manufacture high-precision molds.
Extrusion processing
The cast bar is heated to 400-500℃, and the aluminum is extruded from the mold through an extruder to form a profile with a specific cross-sectional shape.
After extrusion, air cooling or water cooling is used for rapid cooling (such as 6063-T5/T6 alloy requires aging strengthening).
3. Post-processing of profiles
Straightening and alignment
Use hydraulic or mechanical equipment to correct the bending deformation caused by extrusion to ensure that the straightness error of the profile is ≤0.5mm/m.
Artificial aging
Put the profile into an aging furnace for heating (such as 170-200℃) and keep it warm for 2-3 hours to improve hardness and mechanical strength.
4. Surface treatment
Pretreatment
Chemical cleaning to remove surface oil stains, or physical polishing to obtain a smooth substrate.
Anodizing
Generate a dense aluminum oxide film (thickness 5-25μm) in the electrolyte to improve corrosion resistance and wear resistance.
Coloring and sealing
Give silver, black, copper and other appearances through electrolytic coloring or adsorption of dyes, and then seal the membrane pores to enhance performance.
Spraying process
Optional powder spraying (matte/bright) or fluorocarbon spraying (high outdoor weather resistance) to meet diverse decorative needs.
5. Deep processing and customization
Cutting and forming
Sawing or laser cutting to the required length, with an accuracy control of ±0.2mm; complex shapes are formed by CNC bending or rolling.
Drilling and tapping
Processing straight holes, stepped holes or threaded holes, suitable for bolts, nuts and other connectors.
Welding and assembly
Connect special structural parts by argon arc welding or friction welding, and complete the frame assembly with angle codes and connectors.
6. Quality inspection and packaging
Dimension detection
Use calipers and three-coordinate measuring machines to verify profile tolerances (such as wall thickness ±0.1mm).
Performance testing
Tensile strength, hardness (such as Webster hardness ≥8HW) and corrosion resistance (salt spray test ≥1000 hours) testing.
Packaging and shipment
Film is applied to protect the surface, and wooden boxes or pallets are used for packaging to avoid scratches during transportation.
Core Points of the Process
Customized Production: From mold design to surface treatment, everything can be adjusted according to demand, supporting non-standard cross-sections and special functions (such as thermal insulation and photovoltaic slots).
Precision Control: The precision of extrusion and processing must reach ±0.1mm to ensure assembly compatibility.
Green Process: Smelting waste gas treatment and wastewater recycling meet environmental protection standards.