The most important thing for composite aluminum foil products is to keep the equipment hygienic. Each guide roller must be cleaned very clean, otherwise it is easy to have appearance defects, such as small bubbles.

Regarding the problem of bubbles or dots during lamination, one possibility is that the glue reacts with the ink or solvent to generate small bubbles. Due to the characteristics of the material, the air bubbles cannot be released, and small bubbles are formed.

Another possibility is that the glue slowly shrinks to form small dots due to lack of initial tack when applied, and gradually bulges to form small dots.

How to solve the problem of composite aluminum foil?

In these cases, we must first choose the appropriate glue to match the ink, and at the same time keep the composite roller operating at a lower temperature. After getting off the machine, place the material in an environment of 15~20℃ for 2~5 hours, perform secondary leveling, and then proceed to the next step. Process compounding. The winding tension should be as high as possible, and it would be better to wrap several turns of stretch film on the surface of the film roll. During the composite process, try to reduce the speed as much as possible and keep it at 120~150m/min. The composite aluminum plating or AL//PA layer can increase the speed appropriately according to the situation.

Another situation where bubbles appear is due to the influence of the printing layout. When the printing layout is uneven, the winding cannot be tightened, resulting in loose areas that cannot be leveled for a second time, and glue spots or bubbles will occur. So try not to choose hollow layout lamination.

Composite these structures must ensure the environmental conditions of the workshop, and the corresponding temperature and humidity are very important for the composite effect.