How to judge the quality of aluminum beading?
1. Material and appearance inspection Aluminum type and purity Native aluminum verification : High-quality aluminum strips should use primary aluminum (such as 6063-T5/T6), the cross-section color is uniform and silvery white, without dark spots or impurities, and inferior products are mostly recycled aluminum and dark in color . Wall thickness measurement : The wall thickness of the main profile must be ≥1.8mm (new national standard), and the wall thickness of the beading is recommended to be ≥1.2mm. Too thin (such as 0.2-0.35mm) may affect the support strength . Surface treatment and appearance The surface should be flat and smooth, without scratches, oil stains or oxidation spots, and the surface cleanliness can be tested by wiping with alcohol . The thickness of the anodized film must be ≥15μm, and it is recommended to superimpose a nano-coating in coastal areas to enhance corrosion resistance . 2. Process and structure inspection
Process verification
Hollow aluminum strip process: Check whether it is a high-frequency welding integrated bending process (no splicing seams). Splicing aluminum strips can easily cause air leakage or glass displacement.
Insulation strip material: Broken bridge aluminum strips should be matched with nylon PA66 insulation strips, and PVC materials should be avoided.
Section and size adaptability
The cross-sectional shape of the strip (such as U-shaped, L-shaped) needs to match the thickness of the glass. Too narrow may cause sealing failure, and too wide increases costs.
Tolerance control: The matching tolerance between the strip and the window frame should be ≤±0.5mm, and it needs to be flat and seamless after installation.
3. Sealing performance test
Strip matching test
The matching sealing strip should be made of EPDM rubber (EPDM). Through the tensile test: high-quality strips are highly elastic and not easy to break, while inferior strips are prone to white marks or yellowing.
Sealing verification: After installation, you can use A4 paper to clip the gap of the pressure strip. If it is easily pulled out, the seal is unqualified.
Weather resistance evaluation
Exposure test: After assembling the pressure strip and the rubber strip, expose them to the sun for 48 hours to observe whether there is deformation, hardening or oil seepage.
High and low temperature cycle test: simulate the environment of -20℃ to 70℃, and check whether the joint between the rubber strip and the aluminum strip is cracked.