Analysis of aluminum profile production links and standards
I. Core production links
Melting and casting process:
Proportioning and smelting: According to the target alloy grade, the aluminum ingots and alloy elements are accurately proportioned, and the induction furnace or natural gas smelting furnace is used to heat to 700-750℃ for melting, and degassing and slag refining are carried out simultaneously to ensure the purity of the aluminum liquid.
Casting and homogenization treatment: The molten aluminum liquid is cooled into round cast bars through a deep well casting system, and treated in a homogenizing furnace (temperature 500-550℃) to eliminate internal stress and improve subsequent extrusion.
Extrusion molding
Mold making: The mold is designed using CAD/SOLIDWORKS, and high precision is ensured by lathe processing, wire cutting die hole, and nitriding treatment (hardness up to 53-54HRC).
Heating and extrusion parameters: The aluminum bar is heated to 450-500℃, the mold is preheated to 480℃, and formed at a speed of 0.5-5 meters/minute through a 5000-12000 ton extruder. After extrusion, it is water-cooled to shape and stretched and straightened (tolerance ±0.5mm). Surface treatment
Anodizing: After pretreatment (alkaline washing and degreasing), a 5-25μm oxide film is generated in a sulfuric acid electrolyte, and the sealing treatment enhances corrosion resistance. It can be customized in silver white, champagne color, etc. Spraying process: Outdoor materials are sprayed with fluorocarbon (film thickness ≥30μm), and the salt spray test must be 3000 hours without corrosion. Aging strengthening
After extrusion, the profile is kept in an aging furnace at 200-220℃ for 2-3 hours to increase the hardness to T5/T6 state (6061-T6 tensile strength ≥290MPa)