The 6061-T651 aluminum alloy supplied by GNEE is primarily composed of aluminum, with magnesium (Mg) and silicon (Si) as its main strengthening elements. Smaller amounts of copper (Cu), chromium (Cr), manganese (Mn), iron (Fe), zinc (Zn), and titanium (Ti) are also included, giving the alloy a well-balanced combination of strength, corrosion resistance, and machinability. These properties make it widely used in applications such as aircraft components, bicycle frames, precision fittings, and other structural parts. The "T651" temper designation indicates that the material has been solution heat-treated, stress-relieved by stretching, and then artificially aged to optimize mechanical performance.
Chemical Composition (Typical Limits)
Aluminum (Al): approx. 95.8–98.6% (balance)
Magnesium (Mg): 0.8–1.2%
Silicon (Si): 0.4–0.8%
Copper (Cu): 0.15–0.40%
Chromium (Cr): 0.04–0.35%
Manganese (Mn): ≤0.15%
Iron (Fe): ≤0.70%
Zinc (Zn): ≤0.25%
Titanium (Ti): ≤0.15%
6061-T651 Key Features
High Strength: 6061-T651 aluminum has an impressive tensile strength of 310 MPa and a yield strength of 276 MPa, making it an ideal material for high-stress applications.
Weldability: This alloy is well-known for its exceptional weldability, making it a popular choice for applications that need seamless joining or welding.
Corrosion Resistance: With solid corrosion resistance, 6061-T651 aluminum plates perform well in difficult environmental conditions, demonstrating their longevity over time.
Machinability: 6061-T651's exceptional machinability allows for easy shape and fabrication of complex designs, making it a versatile material for aerospace components.
6061 T6 vs. 6061 T651 Temper
Both tempers use the same base alloy, but T651 includes an additional stretching step after heat treatment to relieve internal stress. This improves dimensional stability and toughness, making the T651 temper especially suitable for aluminum plates and forged products supplied by GNEE.

Difference Between T6 and T651 – T651 vs. T6 Temper
T6 and T651 are two commonly used -T tempers for aluminum alloys, frequently seen in materials such as 6061-T6 and 7075-T6 supplied by GNEE.
T6 represents a condition where the alloy has undergone solution heat treatment followed by artificial aging. When dimensional stability and elastic recovery are not critical factors, the T6 temper is a suitable and efficient choice.
T651, on the other hand, involves solution heat treatment, stress relief by controlled stretching, and then artificial aging. For components that demand high precision, the T651 temper is preferred because it minimizes elastic recovery after machining and helps maintain dimensional accuracy.
Key Differences Between T6 and T651 for 6061 Aluminum Plate
The main distinction is that 6061-T6 retains higher internal stress, making it more prone to deformation during machining.
The -T6511 temper is a variant of the T6 series in which internal stresses are significantly reduced, making it more suitable for precision machining.
Differences between -T6, -T651, -T6510, and -T6511 tempers become apparent during machining: stress-relieved conditions provide better stability. When a CNC-machined part undergoes processes such as turning or milling, various forces act on the workpiece. Even if the part appears unchanged while external forces are applied, once the forces are removed, the internal stress causes elastic recovery, leading to dimensional variation.
During aluminum plate production, heat and extrusion create uneven density between crystals. This unreleased energy accumulates inside the metal as internal stress.
Application of T651 Temper
The T651 temper is ideal for thick plates, rolled or cold-finished bars, die forgings, forged rings, or rolled rings that have been solution heat-treated or cooled from high-temperature forming processes. These products are not straightened after stretching, ensuring minimal distortion and excellent dimensional stability-qualities essential in precision manufacturing applications supported by GNEE.