How the Three Alloys Differ
6061, 7075 and 6063 are heat-treatable alloys, so strength is developed by solution treatment followed by artificial ageing. 6063 is a low-strength, high-extrudability alloy used where surface finish and anodising response matter more than load capacity. 6061 delivers a balanced combination of strength, weldability and corrosion resistance at moderate cost, and is the default choice for machined fittings and structural brackets. 7075 is the highest-strength of the three and is selected where weight saving justifies its lower corrosion resistance and higher cost.
Composition Limits and Applicable Standards
Extruded bar and rod are ordered to ASTM B221/B221M; rolled or cold-finished bar to ASTM B211/B211M. Equivalent references are GB/T 3191, JIS H4040 and EN 755-2, the last of which tabulates mechanical properties for extruded rod, bar, tube and profiles.
| Element, % | 6063 | 6061 | 7075 |
|---|---|---|---|
| Mg | 0.45-0.9 | 0.8-1.2 | 2.1-2.9 |
| Si | 0.20-0.6 | 0.40-0.8 | 0.40 max |
| Cu | 0.10 max | 0.15-0.40 | 1.2-2.0 |
| Cr | 0.10 max | 0.04-0.35 | 0.18-0.28 |
| Zn | 0.10 max | 0.25 max | 5.1-6.1 |
Mechanical Properties by Temper
| Material | Typical tensile strength | Typical yield strength | Typical use |
|---|---|---|---|
| 6063-T5 | about 185 MPa | about 145 MPa | Architectural profiles, trim, frames |
| 6061-T6 | about 310 MPa | about 275 MPa | Machined brackets, fixtures, general structural |
| 7075-T6 | about 570 MPa | about 505 MPa | High-load aerospace and sporting components |
| 7075-T73 | about 505 MPa | about 435 MPa | High-strength parts needing stress-corrosion resistance |
These are typical published values for the tempers listed and are given for guidance only; released material must meet the minimum properties stated in the standard the order is placed against.
Size Range, Tolerance and Surface
Round bar is commonly supplied from small diameters up to a few hundred millimetres, in random or fixed lengths such as 2 m, 3 m and 6 m, with flat bar, square bar and hexagonal bar produced to the same alloy and temper. Dimensional tolerance and straightness limits depend on the standard and the production route: extruded bar tolerances are tabulated in ASTM B221/B221M and EN 755-3, while cold-finished bar is held to tighter limits. Surface is normally mill finish, with bright drawn finish available where a machined appearance is not required.
Machining, Finishing and Inspection
All three alloys machine readily, with 6061 giving the best balance of finish and tool life; 7075 machines cleanly but is more sensitive to stress corrosion in exposed service. Anodising response is best on 6063 and 6061, and any anodic coating thickness should be agreed with the finished diameter because the coating grows outward and inward. Inspection covers dimensional checks, straightness, ultrasonic or dye penetrant examination where specified, and a mill certificate linking the heat number to chemistry and mechanical results. Buyers should state the specification revision, temper and inspection class on the order to avoid material that is dimensionally correct but unreleasable.
Frequently Asked Questions
Q: Which alloy should be chosen for a machined bracket?
A: 6061-T6 is the usual choice, since it combines good strength, machinability and corrosion resistance at moderate cost.
Q: When is 7075 preferred over 6061?
A: When the highest strength-to-weight ratio is required; the T73 temper is specified where stress-corrosion resistance in exposed service is also needed.
Q: Is 6063 suitable for structural loads?
A: It is generally used for architectural and trim profiles; where load capacity governs, 6061-T6 is normally substituted.
Q: Which standards cover aluminum rod and bar?
A: ASTM B221/B221M for extruded bar and rod, ASTM B211/B211M for rolled or cold-finished product, with GB/T 3191, JIS H4040 and EN 755-2 as equivalent national references.
Q: Do anodic coatings change the diameter?
A: Yes. The coating grows partly inward and partly outward, so the final diameter must be allowed for when the coating thickness is specified.
Q: Can these alloys be welded?
A: 6061 and 6063 weld readily with matching filler; 7075 is not normally welded because of cracking and loss of properties.