0.5 mm to 3 mm 5083, 5754 and 5052 Aluminum Alloy Sheet

Dec 17, 2025

Leave a message

What Separates the Three Alloys

5083, 5754 and 5052 are all magnesium-bearing non-heat-treatable alloys, so they gain strength by strain hardening rather than by solution treatment. The magnesium content sets the strength: 5052 carries 2.2-2.8 %, 5754 carries 2.6-3.6 % and 5083 carries 4.0-4.9 %. Higher magnesium raises strength and improves resistance to seawater, but it also narrows the welding window and increases the tendency to sensitisation if the material is held at elevated temperature for long periods.

Thin sheet in these grades is ordered to ASTM B209/B209M, which lists permissible thickness variation and minimum mechanical properties for each temper. Marine plate in 5083 is additionally covered by ASTM B928. National equivalents appear in EN 485-2, which tabulates mechanical properties for sheet, strip and plate.

Composition and Typical Properties

Property 5052 5754 5083
Magnesium, % 2.2-2.8 2.6-3.6 4.0-4.9
Manganese, % 0.10 max 0.50 max 0.40-1.0
Chromium, % 0.15-0.35 0.30 max 0.05-0.25
Typical tensile strength about 230 MPa in H32 about 220 MPa in H22 about 305 MPa in H116
Typical yield strength about 195 MPa in H32 about 160 MPa in H22 about 215 MPa in H116

The figures shown are typical values for the tempers named, not guaranteed minimums; acceptance is against the minimum properties tabulated in the applicable standard for the ordered form, temper and thickness.

Temper Selection for Thin Sheet

Temper designations follow the EN 515 system. H111 and H112 indicate a lightly strain-hardened or as-rolled condition and are the usual choice for parts that will be formed heavily, because they retain the most ductility. H22 and H32 are quarter-hard tempers suitable for general fabrication, panel work and brake forming. H116 and H321 are stabilised tempers used in marine service, where resistance to intergranular attack after long exposure at mildly elevated temperature matters.

For 0.5 mm to 3 mm material, the temper rather than the alloy often decides whether a bend will crack. A tight bend radius in a hard temper can fail even though the alloy itself is perfectly weldable.

Fabrication and Application Notes

All three alloys weld well by the gas tungsten arc and gas metal arc processes using a matching filler, and they are readily cut by shear, laser and waterjet. Springback increases with temper, so tooling for H32 or H116 sheet must be set for a larger tool radius than for H111. Surfaces are supplied mill finish, and may be brushed, anodised or embossed; anodising on high-magnesium grades produces a darker, less transparent coating than on 5052.

Typical uses at these gauges include boat hull and deck components, tank and silo panels, road and rail body panels, pressure-vessel internals where permitted, and general sheet-metal fabrication where weight and corrosion resistance both count.

Frequently Asked Questions

Q: Which of the three alloys is strongest?
A: 5083, because its higher magnesium content and manganese addition give the highest strength of the three; 5052 is the lowest and 5754 sits between them.

Q: Which temper should be chosen for tight bends?
A: A soft or lightly hardened temper such as H111 or H112, since springback and cracking risk both rise as strain hardening increases.

Q: Can 5083 be used outdoors in marine air?
A: Yes, and stabilised tempers such as H116 are normally specified for marine structures to resist intergranular attack.

Q: Are these alloys heat treatable?
A: No. They are non-heat-treatable, so strength comes from strain hardening, not from solution treatment and ageing.

Q: What standard applies to thin sheet of these grades?
A: ASTM B209/B209M for sheet and plate, with EN 485-2 as the equivalent European tabulation of mechanical properties.

Q: Does anodising work on 5083?
A: It does, but the coating is darker and less transparent than on 5052 because of the higher magnesium content.