Production Process of Knurled Aluminum Rod

May 13, 2025

Leave a message

1. Raw material preparation and casting
Alloy ratio and smelting
The raw materials are electrolytic aluminum ingots or recycled aluminum materials, and the alloy elements (copper, magnesium, zinc, etc.) are accurately proportioned according to the needs (such as 6061, 7075 and other grades);
The natural gas furnace is used to heat to 700-750℃, and the aluminum liquid is uniformly composed by electromagnetic stirring or mechanical stirring, and degassing and slag refining are carried out simultaneously.
Continuous casting aluminum rod
The refined aluminum liquid is poured into round aluminum rod billets through a continuous casting machine, with a diameter range of Φ100mm to Φ300mm, and the cooling rate is controlled at 10-20℃/min to reduce internal defects;
The ingot needs to be homogenized (temperature 480-500℃ for 4-6 hours) to eliminate intracrystalline segregation and improve processing performance.
2. Extrusion and pre-processing

Mold design and preheating
The mold uses H13 hot-working steel CNC engraved diversion holes and welding chambers, and the working belt is electrospark machined and nitrided (hardness reaches 53-54HRC) to increase life;
Preheat the mold to 400-450℃, and heat the aluminum rod to 410-500℃ (low temperature high speed/high temperature low speed rules are suitable for different alloys).
‌Extrusion and straightening
The aluminum rod is formed in an 800-2500 ton extruder, and the alloy strengthening phase is fixed by air cooling quenching (cooling rate ≥180℃/min);
After extrusion, the profile is eliminated by a tension straightener to eliminate bending, and the straightness error is ≤0.5mm/m.
3. ‌Core Technology of Knurling Process‌
‌Knurling Tool and Clamping‌
Use single or double knurling tool (module 0.3-0.8mm), the tool material is high-speed steel HSS or carbide, and it is strictly vertically aligned with the axis of the aluminum rod;
The workpiece needs to be fixed by a spring chuck or hydraulic clamp to avoid the deviation of the texture caused by processing vibration.
‌CNC knurling operation‌
Initial embossing stage: the tool cuts into the surface of the aluminum rod at a speed of 200-400rpm, directly pressing into the depth of 0.1-0.3mm to form a clear texture;
Knurling stage: the axial feed rate is 0.05-0.2mm/r, ensuring that the mesh or straight line texture is continuous and uniform, and the tool stays at an angle of 10-15° before retracting to eliminate burrs.
4. Surface treatment and testing
Anodizing and coating
After alkaline washing and acid etching, the knurled aluminum rod is anodized in sulfuric acid electrolyte (voltage 12-18V) to form a 10-25μm oxide film;
Electrophoretic coating (E-Coating) or powder spraying (such as RAL color card customized color) can be selected to improve corrosion resistance and appearance texture.
Quality inspection standards
Full-size inspection: caliper measures diameter tolerance (ISO 2768-m grade), projector verifies knurling depth and texture uniformity;
Performance test: salt spray test ≥500 hours to verify corrosion resistance, hardness tester detects oxide film microhardness (≥300HV).
5. Key points of process optimization
Tool loss control: The knurling tool edge needs to be sharpened after processing 500-800 pieces to avoid blurred lines or aluminum sticking to the tool;
Coolant selection: Water-based cutting fluid (such as 5% emulsion) can simultaneously cool down and reduce aluminum chip adhesion;
Customized adaptation: Combined with CAD/CAM software to optimize the knurling path and support the composite processing needs of special-shaped shafts (such as eccentric shafts).

10006

Production process of knurled aluminum rod