Extruded aluminum extrusion stripe shortcomings more varieties, the composition of the elements are also more chaotic, today we come to analyze the cause of the composition of the conflict pattern and the solution. Mold every time the light mold on the machine after kneading, the texture can not be one-to-one correspondence, there are light and heavy.
The main reason in the kneading process, the profile out of the mold hole in the moment and the work of the belt tightly together, constituting a pair of hot state of dry conflict vice, and the work of the belt will be divided into two zones - adhesion area and sliding area. In the adhesion zone, the metal point of mass by at least from two aspects of the force effect: conflict force and shear force. When the adhesion area of the metal point of mass by the conflict force is greater than the shear force, the metal point of mass will be adhered to the adhesion area of the work belt on the exterior, and will be the profile of the exterior scratches and constitutes a conflict with the pattern.



Solution 1, adjust the mold work belt exit angle α, so that it is in -1 ° ~ -3 ° range, so that the work belt can reduce the height of the adhesion zone, reduce the conflict force in the area, increase the sliding area; 2, efficient mold nitriding disposal, so that the mold exterior hardness to maintain the HV900 above; work belt appearance of the sulfurized can be reduced to reduce the adhesion zone conflict force, reduce the conflict pattern.