The heat-treatment process of aluminum alloys is the key to unlocking their strength, corrosion resistance, and dimensional stability. For high-demand applications such as automotive and aerospace components, optimizing heat-treatment parameters can extend service life by over 30%. Below is a core technology and application guide:
T6 Treatment: Peak Strength
Process: Solution treatment at 480–500 °C followed by water quenching, then artificial aging at 180 °C for 8 h. This yields a tensile strength exceeding 570 MPa for 7075-T651 alloy, used in aircraft wing beams and EV crash-protection beams.
Key Point: Keep quench-transfer time under 10 s to prevent β-phase coarsening.
T7 Over-Aging: Stress-Corrosion Resistance
Process: Increase aging temperature to 230–250 °C, sacrificing 5–8 % of peak strength in exchange for superior stress-corrosion performance. 6061-T7 alloy is ideal for ship decks and chemical-reactor supports, with salt-spray resistance exceeding 15 years.
T5 Natural Aging: Rapid Die-Casting Solution
Process: Allow natural aging at 20 °C for 5–10 days immediately after low-pressure die casting. ADC12 motor housings achieve a yield strength of 240 MPa, reducing cycle time by 30 % versus traditional treatments.
Multi-Stage Aging: Dimensional-Stability Assurance
Process: Two-stage aging-120 °C for 4 h, then 170 °C for 8 h-refines grain structure and relieves 75 % of residual stress. 2024-T351 alloy parts (e.g., precision optical brackets) maintain flatness within 0.1 mm/m.
GNEE Group Heat-Treatment Solutions
Process Library: Over 20 optimized heat-treatment cycles (T4, T5, T6, T7) for alloys including 7075, 6061, and 2024
Residual-Stress Mapping: Dual verification by XRD and drilling methods to fine-tune treatment curves
Agile Service: Full sample processing and detailed heat-treatment report delivered within 72 hours