8011 Aluminum Alloy Plate: Tempers O, H12 to H22 Explained

Dec 29, 2025

Leave a message

Understanding the 8011 Alloy System

8011 is a non-heat-treatable aluminium alloy whose main additions are iron and silicon, present as fine intermetallic particles rather than as precipitation-strengthening elements. Because it cannot be strengthened by aging, the mechanical properties are set by strain hardening during rolling, which the temper designation records. This makes the temper the single most important specification item when ordering 8011 plate or foil, and the same alloy can be delivered as soft wrapping foil or as stiff, rigid packaging material depending on the temper chosen.

O Temper: Maximum Formability

The annealed O condition is the softest state, with typical tensile strength around 80 to 100 MPa, yield strength near 30 to 40 MPa and elongation of 20 to 25 percent. This combination makes O temper ideal for deep drawing, folding and complex forming operations, which is why household and flexible packaging foil is supplied in O. The material conforms easily around products and survives repeated flexing without cracking, but it is not suited to load-bearing or self-supporting parts.

H12 to H18: The Strain-Hardened Range

As cold work increases, strength rises and ductility falls. H12 is lightly strain hardened, H14 and H16 are intermediate, and H18 is the fully hardened condition produced by about 75 percent cold reduction, reaching tensile strengths of 130 to 150 MPa with elongation down to 3 to 5 percent and yield strength approaching 120 MPa. H18 plate and foil are stiff and hold their shape, which is why they are used for semi-rigid containers, lids, trays and applications where the material must resist buckling.

H22: The Stabilised Half-Hard Condition

H22 describes a partially strain-hardened temper, typically tensile strength of 100 to 120 MPa, produced by cold working followed by a low-temperature stabilising treatment. It offers a practical middle ground: noticeably stiffer than O for handling and stacking, yet still formable enough for bending and light drawing. In packaging, H22 foil and thin plate are used where a balance between rigidity and converting performance is needed, and the stabilising step improves the consistency of the properties over time.

Selecting the Right Temper for Your Application

Choose O for wrapping, deep drawing, lidding and any operation requiring maximum ductility. Choose H18 where the material must be rigid, such as formed containers, end stock and spacers. Choose H14 or H22 for flat panels, covers and general fabrication that need moderate stiffness with some bendability. Specify the alloy, temper, thickness, width and surface requirement with the order, and request mill certificates if the application is regulated, such as food-contact packaging.

FAQ

What is the main difference between 8011-O and 8011-H18?

8011-O is fully annealed, soft and highly formable with low strength, while 8011-H18 is fully strain hardened, about 50 percent stronger but with much lower elongation, making it stiff and rigid.

Why is 8011 used so widely for household foil?

8011 in soft tempers combines good formability, adequate strength for wrapping, corrosion resistance and low cost, which makes it the standard household foil alloy.

Can 8011 be heat treated to make it stronger?

No. 8011 is non-heat-treatable; the only way to raise its strength is cold working, which is what the H tempers represent.

Is 8011 suitable for food contact?

Yes, 8011 foil and plate can be produced to food-contact standards, and it is widely used for food packaging applications. Confirm the relevant compliance documentation with the supplier.

What does the H in H22 mean?

H indicates a strain-hardened temper. The first digit 2 means strain hardened and partially annealed, and the second digit indicates the degree of hardening, in this case a quarter-hard level after stabilising.