Coil Alloys Inside a Beverage Can
A two-piece beverage can is built from more than one alloy. The drawn and wall-ironed body is normally 3104-class aluminum, while the end shell, tab and some closure parts use a higher-magnesium alloy, most often 5182, supplied in a hard temper. 5052 coil appears where a moderate-strength, highly formable and corrosion-resistant strip is required, for example in non-pressure closures, can components, bottles and lids that are not subjected to the highest internal pressure. Because every can part is produced at very high stroke rates, the coil has to deliver consistent strength, gauge and surface quality, batch after batch.
Composition of 5052 and 5182
| Element | 5052 (%) | 5182 (%) |
|---|---|---|
| Mg | 2.2-2.8 | 4.0-5.0 |
| Mn | 0.10 max | 0.20-0.50 |
| Cr | 0.15-0.35 | 0.10 max |
| Fe | 0.40 max | 0.35 max |
| Si | 0.25 max | 0.20 max |
| Cu | 0.10 max | 0.15 max |
| Zn | 0.10 max | 0.25 max |
The magnesium range is the main difference. 5182 carries roughly twice the magnesium of 5052, which raises strength substantially after cold reduction and also increases the alloy's sensitivity to intergranular corrosion if it is held at elevated temperature in service. Limits are published in ASTM B209 / B209M and in the aluminium-magnesium sections of EN 573-3.
Temper, Strength and Downgauging
End and tab stock is normally supplied in H19 (full hard, cold rolled) or H48 (strain hardened and given a stabilizing treatment) tempers so that the same sheet can be formed into shallow shells and tabs and still hold pressure after seaming. Typical room-temperature values for 5182 in a hard temper are roughly 400-430 MPa tensile strength, 350-380 MPa 0.2% proof stress and 3-6% elongation; 5052 reaches roughly 260-290 MPa tensile strength at full hard. The high strength allows the wall and end thickness to be reduced to roughly 0.20-0.28 mm for the end and near 0.24 mm for the body of a standard can, which is where the weight and material cost of the package are won or lost.
Dimensional and Surface Requirements
Three coil properties drive can-line yield. Gauge tolerance is held much tighter than general sheet tolerances in ASTM B209, typically within a narrow percentage of nominal across the full coil length, because a heavy spot becomes a broken shell in the press. Earing behaviour must be controlled, since an unbalanced texture produces ears on the drawn shell and forces extra trim. Surface cleanliness matters equally: residual rolling oil, fines and inclusions cause pin-holes, blisters and lacquer faults, so coil for can stock is supplied degreased, filtered and often lightly oiled to a controlled film weight. Coil is usually delivered with an inner diameter of 508 mm or 610 mm, with widths matched to the blanking or drawing line.
Standards, Testing and Packing
Coil is ordered to ASTM B209 / B209M or EN 485-2, with chemistry checked against the same standard and dimensional tolerances taken from the corresponding part of the specification. For 5xxx alloys used in wet or hot service, intergranular corrosion resistance can be verified by the nitric acid mass loss test in ASTM G67. Typical inspection on delivery covers chemistry, tensile and elongation on each lot, earing or texture check on the first coil, gauge profile, width, camber, and a lacquer adhesion trial before the coil is released to a can line. Packaging uses eye-to-sky or eye-to-wall orientation with moisture barrier wrap and edge protection to avoid transit damage.
Frequently Asked Questions
Q: Which alloy is standard for beverage can ends?
A: A high-magnesium alloy of the 5182 type is the mainstream choice for end shells and tabs, because its strength after full-hard rolling allows thin, pressure-tight ends.
Q: Why is 5052 used instead of 5182 for some can parts?
A: 5052 is easier to form and more tolerant of bending and deep drawing, so it suits non-pressure closures, lids and components where maximum strength is not required.
Q: What thickness tolerance is realistic for can stock?
A: Suppliers normally hold gauge to a fraction of the general tolerance allowed by ASTM B209, since consistent thickness is essential for shell forming and for material cost control.
Q: Does coil for can stock need to be oiled?
A: Yes, in most cases a thin, controlled rolling or forming lubricant film is applied after degreasing, and its weight and uniformity are agreed with the customer because it affects lacquer adhesion.
Q: Can 5182 coil be welded after forming?
A: The can is a seamed and adhesive-bonded product rather than a welded one, but where welding is used the high-magnesium alloy should be joined with 5356 or 5556 filler and the joint kept away from prolonged elevated-temperature exposure.
Q: How should coil be stored before use?
A: Keep it in the original moisture-barrier wrap, off the floor, away from condensation, and use the oldest coil first, since surface oxide growth and edge damage increase handling loss over time.